Help support TMP


"3Dprinting Markers" Topic


2 Posts

All members in good standing are free to post here. Opinions expressed here are solely those of the posters, and have not been cleared with nor are they endorsed by The Miniatures Page.

Please remember that some of our members are children, and act appropriately.

For more information, see the TMP FAQ.


Return to the 3Dprinting Markers Article


Areas of Interest

General

Featured Hobby News Article


Featured Link


Featured Ruleset


Featured Showcase Article

GF9 Fire and Explosion Markers

Looking for a way to mark explosions or fire?


Featured Profile Article

Report from ReaperCon 2006 - Part III

The final installment of our ReaperCon report.


Featured Book Review


990 hits since 16 Jun 2017
©1994-2024 Bill Armintrout
Comments or corrections?


TMP logo

Membership

Please sign in to your membership account, or, if you are not yet a member, please sign up for your free membership account.
Waco Joe16 Jun 2017 7:19 a.m. PST

I have had issues from time to time with flat pieces curling up at the ends and I have a heated bed. Using PLA I finally found a sweet spot of using a bed temp of 65 degrees instead of of 55, a nozzle temp of 230 instead of the default 215 and using a 3-5mm brim. The combo of higher temps and brim seem to fix the problem.

Along the line of markers, I integrated a marker holder into some of my movement trays. This tray is designed for holding my WWS figures mounted on 2 inch bases. I am playing around with using All The King's Men rules which calls for figure removal and a status of green/yellow/red. I added a small part to the tray to hold a small die and a unit status indicator.

picture

Nice and simple and I don't have to worry about the markers getting separated from the unit.

Personal logo Editor in Chief Bill The Editor of TMP Fezian16 Jun 2017 8:09 a.m. PST

Nice!